Details
Size Information:
Thickness: 1/4", 3/8", 1/2", 3/4", 1"
Standard Lengths: 54"
Slab Width: 36"
Cut to Size: 2" to 36" in 1/2" increments
Typical Properties:
Compression (to 50% of original) 50-500psi
Water Absorption by Weight Average of closed and open-celled sponge
Compression Set 10% maximum. ASTM Method: ½" samples compressed for 22 hours @ 70°F - 24
hour recovery
Density 30 PCF minimum
Temperature Resistance
Low -40°F
Temperature Resistance High Continuous +180°F
Temperature Resistance High Intermittent +220°F
Accelerated Aging: Good
ASTM Method: 7 days at 158°F-lineal shrinkage maximum 2%)
Flexibility 180° bend without cracking
Tensile Strength (minimum) 25psi
Elongation (minimum) 75%